Grog-Chamotte

Poussière à 45 mailles de briques isolantes
G-26 (2,600 F)
45 mesh sieved dust from G-26 IFBs,

Ball Clay

Na2O 0.2% Al2O3 31.0% SiO2 64.2%
K2O 0.9% TiO2 1.8%
MgO 0.4% Fe2O3 1.2%
CaO 0.4%

Loss On Ignition: 11.2%

EPK (Kaolin)

Na2O 0.1% Al2O3 43.9% SiO2 53.7%
K2O 0.4% P2O5 0.3%
MgO 0.1% TiO2 0.4%
CaO 0.2% Fe2O3 0.9%

Loss On Ignition: 14.0%

Custer spar

Na2O 2.9% Al2O3 17.4% SiO2 69.0%
K2O 10.3% Fe2O3 0.1%
CaO 0.3%


G-200 spar

Na2O 3.1% Al2O3 18.6% SiO2 66.6%
K2O 10.8% Fe2O3 0.1%
CaO 0.8%

Loss On Ignition: 0.2%

Nepheline syenite

Na2O 10.6% Al2O3 23.6% SiO2 60.5%
K2O 4.8% Fe2O3 0.1%
MgO 0.0%
CaO 0.4%

Kona F-4 spar

Na2O 6.9% Al2O3 19.6% SiO2 66.9%
K2O 4.8% Fe2O3 0.0%
MgO 0.1%
CaO 1.7%

Loss On Ignition: 0.2%

Équivalences des feldspaths

Américain = Français

1-Feldspath Potassique Custer = Feldspath ICE 10B (DAM)

2-Feldspath Sodique/ = Feldspath CR 79 (DAM)
Calcique Kona F-4

3-Felspath Potassique/ = Feldspath ICE 10B (DAM)
Calcique G-200

N.B. Le G-200 contient moins d’oxyde de calcium (CaO)
que le Kona F-4.
Mais je n’ai pas trouvé d’équivalence en France; donc
on recommande l’utilisation du Custer partout où
apparaît le G-200.